Yet Another Bulletin Board
Sponsored by: The Fans!


Welcome, Guest. Please Login or Register.
Dec 25th, 2024, 3:59pm

Upcoming Premiere Dates:
Survivor 23, Season premiere
Thursday, September 14 (8:00-9:30 PM, ET/PT) on CBS




Home Home Help Help Search Search Members Members Chat Chat Member Map Member Map Login Login Register Register

| Fantasy Survivor Game | Music Forums | The '80s Server Forums | Shop Online |



Metropolis Reality Forums « Second, the construction method (2) »

   Metropolis Reality Forums
   Amazing Race
   Fantasy Amazing Race Games
(Moderators: JP, Heather, Isle_be_back)
   Second, the construction method (2)
Previous topic | New Topic | Next topic »
Pages: 1  Reply Reply Add Poll Add Poll Notify of replies Notify of replies Send Topic Send Topic Print Print
   Author  Topic: Second, the construction method (2)  (Read 130 times)
qizhen0926
Guest

Email

Second, the construction method (2)
« on: Dec 10th, 2015, 11:13pm »
Quote Quote Modify Modify Remove Remove

(5) flooring
Materials to be rolled upright, label facing up. Will indicate color, volume number, batch number of labels in the obvious place. Different colors, different batches of material should be placed separately.
To avoid color, the same color using a multi-volume construction material, preferably the same batch, by volume number order laying. If you use multiple batches of the same color material, be careful not to color but different batches of the same material tied laying.
Ready for laying the material should be placed in the scene for more than 24 hours, the material memory reduction, the temperature is consistent with the construction site. If edges roll, use a dedicated trimmer cutting process for flash.
Before laying the tile sheet folded in half on a construction site ground, not anti-roll material, or will cause stress. When the web is laid on the adhesive, the stress can cause the formation of bubbles. Folding Department should have some curvature, in order to avoid unnecessary creases, resulting in losses. Before construction, the floor should be cleaned and membrane surface and then scraping gum above the ground floor. It was playing the line according to the door position, pre-coated materials, lofting, cutting cutting.
Apply with a notched knife adhesive (commonly known as glue) to be evenly spread on the ground, for concrete grade absorbent floor, glue-coated 4-5㎡ per liter. Be sure to pay attention to when the glue evenly coated full ground, they can not stay at the uncoated adhesive to glue the corners or uneven. For absorbent ground, glue a few minutes to shop. (Concrete construction method according to the glue manufacturer's instructions).
When laying, the first coil and the second aligned side by side, holding the opposite direction to install. If the irregular edges, you can overlap two material about 5cm. Construction is best to start from the room entrance, so the floor is patchwork at the door. We will try to rely on the web starting wall, if the starting wall uneven, it is best to use a long scriber fit with the wall. There are lines on the floor to try to get the colors aligned grain construction. When cutting, construction materials more reserved than the actual length of 5cm. Walls and materials to hand corner partly covered fully pressed (V-shaped), press corner surface curve (reserved 5cm) reduction. Crop To retain a certain distance from the wall to the location earmarked to cover the baseboard. After pasting the floor, the first floor with a soft wood pressed and extruded flat surface air. Followed by 50 or 70 kilograms of steel pressure roller rolling floor uniformly and timely repair splice case access Alice edges. Floor surface should be wiped off the excess glue.
(6) connected to the joint portion
Grooving and weld must be laid 24 hours after the glue on the floor and then be fully cured. Using a dedicated slot slot along the seams when slotting. For the welding firm, slit through the end should not be recommended for the thickness of the floor grooving depth 2/3 slot can not operate in non-terminal portion, using manual slotted knife in the same depth and width of the slot.
All seams connection, usually using a thermal welding method. Heat welding so that the seam rugged, waterproof and hygienic. Specific welding method steps are as follows:
① Before welding, first remove the tank remaining dust and debris;
② can choose manual or automatic equipment specializing in high quality and with a 5mm fast gun nozzle welding torch welding. Welding torch should be preheated before starting a few minutes, soldering temperature should be set at about 350 degrees -450 degrees Celsius, the heat generated at this time can be simultaneously melted metal and welding rod. After the welding torch nozzle is inserted, the first segment electrode is pressed into the slot one minute, the next move heat gun. Before some of the debris to find the best hands to do some exercises, carefully reflecting electrode, because the welding temperature, the speed and intensity of the use of heat welding results have a direct impact. Welding speed should be appropriate (to ensure welding rod melting), the welding rod extruded into uniform to open a good groove. Solder material must remain parallel with the ground and placed directly on the notch;
③ electrode half when cooled, electrodes Shuhei or monthly type cutter rod above the floor will generally planar portion amputated. After welding cool completely, then use electrodes Shuhei or months electrode type cutting knife cut off the rest of dressing.
(7) the completion of the cleaning again.
Article Source:
รั้วคอ&# 3617;โพสิตในชุมพร
soluciones para pavimentos exteriores
IP Logged
Back to top
Pages: 1  Reply Reply Add Poll Add Poll Notify of replies Notify of replies Send Topic Send Topic Print Print

Previous topic | New Topic | Next topic »

Metropolis Reality Forums » Powered by YaBB 1 Gold - SP 1.3.1!
YaBB © 2000-2003. All Rights Reserved.